Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
News
Home ProductsPermanent Magnet Alloy

Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32

China Suzhou Xunshi New Material Co., Ltd certification
China Suzhou Xunshi New Material Co., Ltd certification
Have been business relationship for 3 years, great partner for Nickel Cobalt Alloy!

—— Daniel Weree

On-time delivery. And support is good and fast.

—— Carolina Fasio

I'm Online Chat Now

Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32

Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32
Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32 Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32 Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32

Large Image :  Cold Drawn Wire Permanent Magnet Alloy Strip Thickness 0.20~1.00 mm 2J32

Product Details:

Place of Origin: China
Brand Name: AIWEN
Certification: ISO 9001:2015
Model Number: 2J32

Payment & Shipping Terms:

Minimum Order Quantity: 30kg
Price: Negotiable
Packaging Details: Plywood case
Delivery Time: 45-50 days
Payment Terms: T/T
Supply Ability: 200 kg per week
Detailed Product Description
Spec: GB/T 14989-2015 Thickness: 0.20~1.00mm
Forms Of Supply: Cold Rolled Strip, Cold Drawn Wire Hc: 23.88 KA/m
Br: 0.75 T Br·Hc: 19.10 KJ/m3
High Light:

cobalt iron alloy

,

magnetic materials

2J32 Permanent-Magnet Alloy Cold Rolled Strip for Recording Material

 

 

A-ONE ALLOY is able to produce 2J32 permenent magnet alloy in forms of wire, strip or per customer requirement.

2J32 is used to make small section permanent magnet and recording material.

 

Forms available: cold drawn wire and cold rolled strip

 

Size range:

Wire diameter: 0.05~3.0mm

Strip thickness: 0.20~1.00mm

 

Chemical composition

Element C Si Mn P S Ni Co V Fe
Weight(%) 0.12 max. 0.50 max. 0.50 max. 0.025 max. 0.020 max 0.70 max. 51.0~53.0 11.8~12.7 Balance

 

Delivery condition: without heat treatment

 

The parts should be heat treated after they are processed to get required magnetic properties.

 

Magnetic properties(after heat treatment)

Form Cold drawn wire Cold rolled strip
Parameter

Hc

(kA/m)

Br

(T)

Br·Hc

(kJ/m3)

Hc

(kA/m)

Br

(T)

Br·Hc

(kJ/m3)

Value 27.86 min. 0.85 min. 23.88 min. 23.88 min. 0.75 min. 19.10 min.

 

Heat treatment

Grade Temperature(°C) Duration(min) Cooling
2J32 580~640 20~60 air cool

 

 