0.05~3.0mm 2J33 Permanent Magnetic Alloy Cold Drawn Wire For Recording Material
Contact me for free samples and coupons.
WhatsApp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xSpec | GB/T 14989-2015 | Diameter | 0.05~3.0mm |
---|---|---|---|
Forms Of Supply | Cold Drawn Wire, Cold Rolled Strip | Hc | 31.84 KA/m |
Br | 0.70 T | Br·Hc | 23.88 KJ/m3 |
Highlight | precipitation hardening alloys,cobalt iron alloy,3.0mm Permanent Magnetic Alloy |
2J33 Permanent-Magnet Alloy Cold Drawn Wire for Recording Material
A-ONE ALLOY is able to produce 2J33 permenent magnet alloy in forms of wire, strip or per customer requirement.
2J33 is used to make small section permanent magnet and recording material.
Forms available: cold drawn wire and cold rolled strip
Size range:
Wire diameter: 0.05~3.0mm
Strip thickness: 0.20~1.00mm
Chemical composition
Element | C | Si | Mn | P | S | Ni | Co | V | Fe |
Weight(%) | 0.12 max. | 0.50 max. | 0.50 max. | 0.025 max. | 0.020 max | 0.70 max. | 51.0~53.0 | 11.8~12.7 | Balance |
Delivery condition: without heat treatment
The parts should be heat treated after they are processed to get required magnetic properties.
Magnetic properties(after heat treatment)
Form | Cold drawn wire | Cold rolled strip | ||||
Parameter |
Hc (kA/m) |
Br (T) |
Br·Hc (kJ/m3) |
Hc (kA/m) |
Br (T) |
Br·Hc (kJ/m3) |
Value | 31.84 min. | 0.70 min. | 23.88 min. | 27.86 min. | 0.60 min. | 18.31 min. |
Heat treatment
Grade | Temperature(°C) | Duration(min) | Cooling |
2J33 | 580~640 | 20~60 | air cool |