Daniel WereeHave been business relationship for 3 years, great partner for Nickel Cobalt Alloy! -
Carolina FasioOn-time delivery. And support is good and fast.
Higher Yield Strength Nickel Cobalt Alloy GH4738 Precipitation Hardened Superalloy
Contact me for free samples and coupons.
WhatsApp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
x| Working Temperature | 815°C | Equal Grades | WASPALOY, GH738 |
|---|---|---|---|
| Density | 8.22g/cm3 | Melting Range | 1330~1360°C |
| Form Of Supply | Hot Rolled Plate, Cold Rolled Plate, Pipe, Strip, Wire, Forging, Casting , Fastner | Product Name | Nickel Cobalt Alloy |
| Highlight | nickel based alloys,cobalt based alloy |
||
GH4738 is a Ni-Cr-Co based precipitation hardened superalloy.
GH4738 has higher yield strength and fatigue resistance during 760°C~870°C.It has good oxidation resistance and corrosion resistance in a gas turbine atmosphere at 870 degree C.It has good ductility and stable properties. It is suitable for making turbine disk, working blade, high temperature fastener, flame tube, shaft and turbine brake.
Chemical composition
| Element | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
| Weight(%) | 0.03~0.10 | 18.0~21.0 | Rem | 12.0~15.0 | 3.50~5.00 | 1.20~1.60 | 2.75~3.25 | 2.00 max |
| Element | B | Zr | Mn | Si | P | S | Cu | |
| Weight(%) | 0.003~0.010 | 0.020~0.080 | 0.10 max | 0.015 max | 0.015 max | 0.015 max | 0.100 max |
The alloys have good oxidation resistance and corrosion resistance in various atmospheres encountered in jet engines or similar working conditions. Continuous operation of the antioxidant temperature up to 1040°C. Intermittent operation of the antioxidant temperature up to 870°C.
Forms of supply
Cold drawn bar
Hot rolled bar
Cold drawn wire
Hot rolled plate
Cold rolled plate
Cold rolled strip
Hot forged bar
Hot fored plate, ring