• Suzhou Xunshi New Material Co., Ltd
    Daniel Weree
    Have been business relationship for 3 years, great partner for Nickel Cobalt Alloy!
  • Suzhou Xunshi New Material Co., Ltd
    Carolina Fasio
    On-time delivery. And support is good and fast.
Contact Person : Allen Sun
Phone Number : +86 18112628895
WhatsApp : +8618112628895

UMCo50 Nickel Cobalt Alloy Thermal Shock Wear Resistance 1380∼1395°C Melting

Place of Origin China
Brand Name XUNSHI
Certification ISO 9001
Model Number UmCo50
Minimum Order Quantity 100kg
Price Negotiable
Packaging Details Plywood case
Delivery Time 30-35 days
Payment Terms T/T
Supply Ability 500kg per week

Contact me for free samples and coupons.

Whatsapp:0086 18588475571

Wechat: 0086 18588475571

Skype: sales10@aixton.com

If you have any concern, we provide 24-hour online help.

x
Product Details
Composition Co-28Cr-21Fe-1Co-1Si-0.9Mn (mass%) Forms Of Supply Forging, Round Bar, Tube
Density 8.05 Melting Temperature 1380∼1395°C
Model UmCo50 Product Name Nickel Cobalt Alloy
High Light

nickel based alloys

,

high temperature nickel alloys

,

UMCo50 Nickel Cobalt Alloy

Leave a Message
Product Description

UMCo50 with Excellent Thermal Shock Resistance and Wear Resistance

 

Main Features
UMCo50 is a heat-resistant cobalt alloy that has excellent thermal shock resistance and wear resistance. It also shows great strength against sulfur-and vanadium-attacks. Another feature is its higher melting point compared to other cobalt base or nickel base heat-resistant alloys. For example, the alloy used for skid rails at a steel mill undergoes regular use at 1,350°C. Thus UMCo50 shows successful results in the application related to heat treatments and furnaces where other alloys could not be used due to their low melting point.

 

Chemical Composition(%)

Element C Si Mn S P Ni Cr Co Mo Fe
Min. 0.05 0.50 0.50 - - 2.00 27.00 48.00 1.00 Blance
Max. 0.12 1.00 1.00 0.020 0.020 2.50 29.00 52.00 1.50 Blance

 

Physical Properties

Specific gravity Melting temperature Electrical Resistivity (25°C) Thermal expansion
(0
1000°C)
Specific thermal conductivity
(22°C)
8.05 1380∼1395°C 82.5Ω•cm 16.8 X 10-6 /°C 0.022cal/cm/sec./°C

 

High temperature corrosion

  Temperature(°C) Time Reduced weight
g/m2 g/m2/hr
Plate (Flat rolled) 1000 144hr 26∼83 0.18∼0.58
Plate (Flat rolled) 1200 144hr 200∼120 0.69∼0.83