Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
News
Suzhou Xunshi New Material Co., Ltd
Home ProductsNickel Cobalt Alloy

Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

China Suzhou Xunshi New Material Co., Ltd certification
China Suzhou Xunshi New Material Co., Ltd certification
Have been business relationship for 3 years, great partner for Nickel Cobalt Alloy!

—— Daniel Weree

On-time delivery. And support is good and fast.

—— Carolina Fasio

I'm Online Chat Now

Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy
Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

Large Image :  Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

Product Details:
Place of Origin: China
Brand Name: AIWEN
Certification: ISO9001
Model Number: GH3536
Payment & Shipping Terms:
Minimum Order Quantity: 50kg
Price: Negotiable
Packaging Details: Plywood case
Delivery Time: 30-35 days
Payment Terms: T/T
Supply Ability: 1000kg per week
Detailed Product Description
Equal Grades: GH536, Hastelloy X, N06002 Melting Range: 1295°C~1381°C
Density: 8.28g/cm3 Magnetic: No
Forms Of Supply: Plate, Strip, Tube, Bar, Forging, Ring, Casting Product Name: Nickel Cobalt Alloy
High Light:

nickel based alloys

,

cobalt based alloy

GH3536 Nickel Based Solid Solution Reinforced Superalloy Hastelloy X

 

 

GH3536 is a Nickel Based Solid Solution Reinforced Superalloy. It is equal to Hastelloy X alloy.

It has good resistance to oxidation and corrosion resistance, under 900 ℃ have moderate to lasting and creep strength, cold and hot working good formability and weldability.

Applicable to the manufacture of aircraft engine combustion chamber components and other high temperature parts, use for a long time under 900 ℃, short-time working temperature of 1080 ℃. In 600 ~ 1200 ℃ high temperature can withstand the stress and resistance to oxidation and corrosion resistance of the alloy. The matrix elements can be divided into iron base superalloy, nickel base superalloy and cobalt base superalloy. According to the preparation process, it can be divided into deformation superalloy, casting superalloy and powder metallurgy superalloy. According to the reinforcement method, there are solid solution enhancement, precipitation enhancement, oxide dispersion enhancement and fiber enhancement (see metal enhancement). High temperature components such as turbine blades, guide blades, turbine discs, high-pressure compressors and combustors for aerospace, naval vessels and industrial gas turbines. It is also used in the manufacture of energy conversion devices such as space vehicles, rocket engines, nuclear reactors, petrochemical equipment and coal conversion

 

Chemical composition

 

Element C Cr Ni Co W Mo Al Ti
Weight(%) 0.05~0.15 20.50~23.00 Rem 0.50~2.50 0.20~1.00 8.00~10.00 0.50 max 0.15 max
Element Fe B Mn Si P S Cu  
Weight(%) 17.00~20.00 0.010 max 1.00 max 1.00 max 0.025 max 0.015 max 0.500 max  

 

Characters of GH3536

  •  Good workability.
  •  At 900 ℃ with medium of lasting and creep strength.
  •  Good oxidation resistance and corrosion resistance.
  •  Suitable for application in a long time of aircraft engine combustor under 900 ℃ and reheater components.
  •  Good welding performance and cold and hot working formability.

Application of GH3536

  •  Industrial and aircraft steam turbine (burner, rectifier, structural cover)
  •  Industrial furnace components, supporting roller, grid plate, ribbon and radiation pipe
  •  Spiral pipes in a petrochemical furnace
  •  High temperature gas cools the nuclear reactor 

Forms and sizes of supply

Plate 0.50~4.0mm

Strip: 0.05~0.80mm

Tube: diameter 4~20mm, wall thickness 1.0~2.0mm

Wire: diameter 0.20~10.00mm

Bar: diameter upto 300mm

Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy 0

Contact Details
Suzhou Xunshi New Material Co., Ltd

Contact Person: Allen Sun

Tel: +8618112628895

Send your inquiry directly to us (0 / 3000)